Show simple item record

dc.contributor.authorSchmitt, E.A.
dc.contributor.authorFlanagan, D.R.
dc.contributor.authorLinhardt, Robert J.
dc.date1993
dc.date.accessioned2022-06-27T17:14:57Z
dc.date.available2022-06-27T17:14:57Z
dc.date.issued1993
dc.identifier.citationDegradation and Release Properties of Poly (D,L-Lactide-co-Glycolide, 50:50) Pellets Fabricated From Three Commercial Polymers, E.A. Schmitt, D.R. Flanagan, R.J. Linhardt, Journal of Pharmaceutical Sciences, 82, 326-329 (1993).
dc.identifier.urihttps://doi.org/10.1002/jps.2600820322
dc.identifier.urihttps://hdl.handle.net/20.500.13015/5983
dc.descriptionJournal of Pharmaceutical Sciences, 82, 326-329
dc.descriptionNote : if this item contains full text it may be a preprint, author manuscript, or a Gold OA copy that permits redistribution with a license such as CC BY. The final version is available through the publisher’s platform.
dc.description.abstractPoly(D,L-lactide-co-glycolide, 50:50) samples of similar molecular weight were obtained from three commercial sources and were characterized by gel permeation chromatography, differential scanning calorimetry, X-ray powder diffraction, viscometry, and proton nuclear magnetic resonance spectroscopy. Pellets were prepared by melt-pressing spray-dried polymer with a 4-mm standard concave punch and die set and a thermostated holder of original design. Amaranth (5% w/w) was incorporated in pellets used for release studies. Degradation and release studies were conducted at 37 degrees C in pH 7.2 phosphate buffered saline. The molecular weights of all polymers were found to decrease continuously after exposure to phosphate buffered saline. All polymers showed two distinct regions of molecular weight decrease. Mass loss experiments for all polymers resulted in sigmoidal curves typical of polymers undergoing bulk hydrolysis. The onset of mass loss (defined as 10% mass loss) was found to differ by as much as 6 days among the three polymers studied. The release studies showed an initial burst of release followed by a period of 15-25 days during which little or no dye was released. A second phase of release followed, lasting approximately 10 days, until all dye was released. The time at which release began slightly preceded the onset of mass loss.
dc.languageen_US
dc.language.isoENG
dc.relation.ispartofThe Linhardt Research Labs Online Collection
dc.relation.ispartofRensselaer Polytechnic Institute, Troy, NY
dc.relation.urihttps://harc.rpi.edu/
dc.subjectBiology
dc.subjectChemistry and chemical biology
dc.subjectChemical and biological engineering
dc.subjectBiomedical engineering
dc.titleDegradation and Release Properties of Poly (D,L-Lactide-co-Glycolide, 50:50) Pellets Fabricated From Three Commercial Polymers
dc.typeArticle
dc.rights.holderIn Copyright : this Item is protected by copyright and/or related rights. You are free to use this Item in any way that is permitted by the copyright and related rights legislation that applies to your use. For other uses you need to obtain permission from the rights-holder(s). https://rightsstatements.org/page/InC/1.0/
dc.creator.identifierhttps://orcid.org/0000-0003-2219-5833
dc.relation.departmentThe Linhardt Research Labs.
dc.relation.departmentThe Shirley Ann Jackson, Ph.D. Center for Biotechnology and Interdisciplinary Studies (CBIS)


Files in this item

FilesSizeFormatView

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record